Горохова Е.И., Демиденко В.А., Еронько С.Б., Родный П.А., Михрин С.Б., Орещенко Е.А. Люминесцентные и сцинтилляционные свойства оптической керамики Gd2O2S:Eu // Оптический журнал. 2010. Т. 77. № 1. С. 65–76.
Gorokhova E.I., Demidenko V.A., Eronko S.B., Rodniy P.A., Mikhrin S.B., Oreshchenko E.A. Luminescence and scintillation properties of Gd2O2S:Eu optical ceramic [in Russian] // Opticheskii Zhurnal. 2010. V. 77. № 1. P. 65–76.
E. I. Gorokhova, V. A. Demidenko, S. B. Eron’ko, E. A. Oreshchenko, P. A. Rodnyĭ, and S. B. Mikhrin, "Luminescence and scintillation properties of Gd2O2S:Eu optical ceramic," Journal of Optical Technology. 77(1), 50-58 (2010). https://doi.org/10.1364/JOT.77.000050
This paper discusses how the dopant concentration and the heat-treatment atmosphere affect the spectral composition of the emission, the thermally stimulated luminescence, and the kinetic damping parameters of ceramic samples of Gd2O2S:Eu. The dependences of the spectral composition of the emission of the ceramic on the dopant and codopant concentration and the excitation energy are established. Ceramic Gd2O2S:Eu possesses high transmittance for an anisotropic material (more than 40% for a thickness of 1.65mm) in the intrinsic-emission region and an overall x-ray-luminescence intensity equal to 150% relative to that for CsI:Tl. The lifetime of the Eu3+ ion in the excited state on the D05 level is no more than 450μs.